What is TPV?
TPV (Thermoplastic Vulcanizate) is made of polymer(PP/PE/PS) and rubber (EPDM, NBR, SEBS, ACM, etc ) with oil, plasticizer, additives, etc.
TPV Properties
- Good elasticity
- Compression deformability resistance
- Anti-Aging
- Wide temperature adaptability, could be used under temperatures -60 C to 135 C
- Good process properties
- Recyclable
- Low bulk density (0.9-0.97)
- Hardness between Shore 25A to Shore 65D
Applications
It is widely used in Automotive, Electrics, Consumer tools, transport tools, construction tools, etc
Main components to get TPV
- Gravimetric feeding system
- High torque twin screw compounder
- Vacuum system
- Melt pump
- Under water pelletizer
COWELL Proposal for TPV Compounding System
Model | Motor kW | L/D | Rotation Speed rpm | Output kg/hr |
CWT52-Plus | 110 | 64 | 600 | 150-180 |
CWT65-Plus | 160 | 64 | 600 | 200-300 |
CWT75-Plus | 250 | 64 | 600 | 400-500 |
CWT95-Plus | 550 | 64 | 600 | 800-1000 |
COWELL Under Water Pelletizing System for TPV
Model | Motor kW | Knife Feed | No.of hole | Heater | Output |
UW200 | 3 | Pneumatic | 18 | Cartridge | 100-250 |
UW300 | 5.5 | Pneumatic | 24 | Cartridge | 200-350 |
UW500 | 7.5 | Pneumatic | 36 | Cartridge | 400-500 |